ERNiCrMo-4
ERNiCrMo-4 can be used for welding nickel-chromium-molybdenum base materials to itself and welding of materials of similar chemical composition, as well as dissimilar material of nickel base alloys, steels and stainless steels.
ERNiCrMo-4 of its high molybdenum content it offers excellent resistance to stress corrosion cracking, pitting, and crevice corrosion, thus it is often used for cladding.
ERNiCrMo-4 often used for groove welding of 9% nickel steels in the production of LGN storage tanks.
Common Names: Oxford Alloy C-276 FM C-276 Techalloy 276
Conformances: AWS A5.14, ASME SFA-5.14, UNS N10276
CHEMICAL COMPOSITION(%)
|
C |
Si |
Mn |
S |
P |
Ni |
Co |
|---|---|---|---|---|---|---|
|
≤0.02 |
≤0. 08 |
≤1.0 |
≤0.03 |
≤0.04 |
Rest |
≤2.5 |
|
W |
V |
Fe |
Cu |
Cr |
Mo |
others |
|
3.0-4.5 |
≤0.35 |
4.0-7.0 |
≤0.5 |
14.5-16.5 |
15-17 |
<0.5 |
WELDING PARAMETERS
|
Process |
Diameter |
Voltage |
Amperage |
Shielding Gas |
|---|---|---|---|---|
|
TIG |
.035” (0.9mm) .045” (1.2mm) 1/16” (1.6mm) 3/32” (2.4mm) 1/8” (3.2mm) |
12-15 13-16 14-18 15-20 15-20 |
60-90 80-110 90-130 120-175 150-220 |
100% Argon 100% Argon 100% Argon 100% Argon 100% Argon |
|
MIG |
.035” (0.9mm) .045” (1.2mm) 1/16” (1.6mm) |
26-29 28-32 29-33 |
150-190 180-220 200-250 |
75% Argon + 25% Helium 75% Argon + 25% Helium 75% Argon + 25% Helium |
|
SAW |
3/32” (2.4mm) 1/8” (3.2mm) 5/32” (4.0mm) |
28-30 29-32 30-33 |
275-350 350-450 400-550 |
Suitable Flux may be used Suitable Flux may be used Suitable Flux may be used |